C51100
C51100
Standard
JIS | DIN | EN | ASTM/UNS/CDA | GB/T |
C5111 | CuSn4 / 2.1016 | CuSn4 / CW450K | C51100 | / |
Merit
CuSn4 belongs to the copper-tin alloys. In the group of phosphor bronzes CuSn4 CuSn4 is the alloy with the highest electrical conductivity.It provides an excellent combination of strength, excellent formability and hardness. It has a good electrical conductivity and corrosion resistance.
Applications
Miniaturized Connectors, Contact Springs, Relais Springs, Terminals, Switch Parts Fuse Clips, Electronic Connectors,etc.
Cu | Remainder |
Sn | 3.5-4.5 |
P | 0.01-0.4 |
Request a Quote
Temper | Tensile Strength(Mpa) | Yield Strength(Mpa) | Elongation (%) | Hardness(HV) | Bending Test(90°)GW | Bending Test(90°)BW |
R290 | 290-400 | max. 190 | min. 40 | 70-100 | 0 | 0 |
R390 | 380-490 | min. 320 | min. 11 | 115-155 | 0 | 0 |
R480 | 480-570 | min. 440 | min. 4 | 150-180 | 0 | 0 |
R540 | 540-630 | min. 510 | min. 3 | 170-200 | 0.5 | 1.5 |
R610 | min. 610 | min. 580 | – | min. 190 | 2 | 6 |
Physical properties of the above materials are conventional performance indicators.If you have some special requirements,(for example property and tolerance).please contact Kinmachi Company directly,we will give you professional assessments and answers.
Density (g/cm³) | 8.85 |
Electrical conductivility IACS%(20℃)* | 21 |
Modulus of elasticity (KN/mm²) | 120 |
Coefficient of thermal expansion 10-6/K | 17.8 |
Thermal conductivity W/(m*K) | 100 |
*value for the lowest temper class
JIS: C5111
DIN: CuSn4 / 2.1016
EN: CuSn4 / CW450K