HASTELLOY C276
HASTELLOY C276
Standard
JIS | DIN | EN | ASTM/UNS/CDA | GB/T |
NW0276 | NiMo16Cr15W / 2.4819 | / | N10276 | / |
Merit
C276 is a Ni-Cr-Mo alloy with excellent corrosion resistance in both oxidizing and reducing atmospheres. In this alloy, carbide precipitation in the heat affected zone (HAZ) is suppressed and corrosion resistance is improved by reducing the contents of C and Si.
Applications
Bellows, Heat exchangers, centrifugal separators, driers, reaction vessels, salt manufacturing plants, flue gas desulfurization plants.
JIS: NW0276
DIN: NiMo16Cr15W / 2.4819
- Sophia
- +86-21-62968227
- sophia@kinmachi.com
- candy_wu@kinmachi.com
Ni | Remainder | C | max. 0.01 |
Mo | 15-17 | Si | max. 0.08 |
Cr | 14.5-16.5 | Mn | max. 1.0 |
Fe | 4.0-7.0 | V | max. 0.35 |
W | 3.0-4.5 | P | max. 0.04 |
Co | max. 2.5 | S: | max. 0.03 |
Temper | Tensile Strength(Mpa) | Yield Strength(Mpa) | Elongation (%) | Hardness(HV)
Brinell |
Bending Test(90°)GW | Bending Test(90°)BW |
HASTELLOY C276 | min. 690 | min. 283 | min.40 | max. 100HRB | – | – |
Physical properties of the above materials are conventional performance indicators.If you have some special requirements,(for example property and tolerance).please contact Kinmachi Company directly,we will give you professional assessments and answers.
Density (g/cm³) | 8.9 |
Electrical Resistivity (μ Ω.cm) | 130 |
Melting Range (℃) | 1325-1369 |
Coefficient of thermal expansion 10-6/K | 12.1 |
Thermal conductivity W/(m*K) | 9.9 |
*value for the lowest temper class