C26800
C26800
Standard
JIS | DIN | EN | ASTM/UNS/CDA | GB/T |
C2680 | CuZn33 2.0280 | CuZn33 / CW506L | C26800 | / |
Merit
Good resistance to fresh water,neutral or alkaline solutions Not resistant to:acids,hydrous sulphur compounds,hydrous ammonia in non-stress-relieved condition.
Applications
Main material for general electrical applications,Jewellery and metal goods Deep drawn parts Stamped parts connectors.
Cu | 63.5-68.0 |
Fe | max. 0.1 |
Pb | max. 0.05 |
Zn | Remainder |
Request a Quote
Temper | Tensile Strength(Mpa) | Yield Strength(Mpa) | Elongation (%) | Hardness(HV) | Bending Test(90°)GW | Bending Test(90°)BW |
R280 | min. 275 | max. 170 | min. 35 | 55-95 | 0 | 0 |
R350 | 350-440 | min. 170 | min. 23 | 85-145 | 0 | 0 |
R420 | 410-540 | min. 300 | – | 105-175 | 0 | 0 |
R500 | 500-620 | min. 450 | – | 145-195 | 0.5 | 0.5 |
Physical properties of the above materials are conventional performance indicators.If you have some special requirements,(for example property and tolerance).please contact Kinmachi Company directly,we will give you professional assessments and answers.
Density (g/cm³) | 8.5 |
Electrical conductivility IACS%(20℃)* | 26 |
Modulus of elasticity (KN/mm²) | 112 |
Coefficient of thermal expansion 10-6/K | 19.9 |
Thermal conductivity W/(m*K) | 121 |
*value for the lowest temper class
JIS: C2680
DIN: CuZn33 2.0280
EN: CuZn33 / CW506L
UNS: C26800
- Sophia