C27200

Standard

JIS DIN EN ASTM/UNS/CDA GB/T
C2720 CuZn37 2.0321 CuZn37 / CW508L C27200 /

Merit

It has good mechanical properties and high strength and plasticity, and can well withstand cold and hot pressure processing.

 

Applications

Hardware, daily necessities, screws and other parts

Cu 62-65
Zn Remainder

Request a Quote

Temper Tensile Strength(Mpa) Yield Strength(Mpa) Elongation (%) Hardness(HV) Bending Test(90°)GW Bending Test(90°)BW
R300 285-370 max. 180 min. 38 55-95 0 0
R350 340-440 min. 170 min. 19 95-125 0 0
R410 410-490 min. 300 min. 8 120-155 0 0
R480 480-560 min. 430 min. 3 150-180 0 0.5
R550 550-640 min. 500 170-200 1 2
R630 min. 630 min. 600 min. 190 2 6

Physical properties of the above materials are conventional performance indicators.If you have some special requirements,(for example property and tolerance).please contact Kinmachi Company directly,we will give you professional assessments and answers.

Density (g/cm³) 8.45
Electrical conductivility IACS%(20℃)* 24
Modulus of elasticity (KN/mm²) 110
Coefficient of thermal expansion 10-6/K 20.2
Thermal conductivity W/(m*K) 121

*value for the lowest temper class